Gas Pool Coupled Activating TIG Welding Method with Coupling Arc Electrode

Yong Huang et al · KeAi Communications Co., Ltd · 2018

Accesso aperto disponibile
Lettura rapida. Controlla i dati essenziali della risorsa e accedi al contenuto con il pulsante principale. La scheda mostra solo le informazioni necessarie per identificare, citare e aprire l’opera.

Accesso alla risorsa

Apri il contenuto dall’opzione principale o scegli un’altra fonte disponibile.

DOAJ DOAJ Articles
Entrar por DOAJ
Accesso principale

Accesso aperto disponibile

Recurso identificado como acceso abierto, sin confirmar automáticamente si es texto completo directo.
Apri risorsa

Riepilogo

Descripción general del contenido del recurso.

Abstract Gas pool coupled activating TIG (GPCA-TIG) welding put forward in-house can dramatically enhance weld penetration of TIG welding through introducing active element oxygen to reverse the Marangoni convection flow in the molten pool. In order to further improve the welding productivity, the normal solid tungsten electrode is replaced by a kind of coupling arc electrode. The changes of arc pressure distribution along anode surface and the weld appearance were evaluated. On this basis, the dependences of weld shape characterized with weld depth, width and undercut on the main welding parameters were discussed. The results indicate, the substitution of coupling arc electrode can lead to an obvious decrease of arc pressure. Compared to hollow tungsten electrode and twin tungsten electrodes, the coupling arc electrode is much easier to manufacture and has more compacter structure. Combined with the symmetric distribution of arc pressure in different directions, this electrode has extensive adaptability. In the GPCA-TIG welding with coupling arc electrode, both the substitution of coupling arc electrode and the introduction of outer active gas oxygen can reduce the possibilities of producing humping bead and undercut. Their joint action makes this welding method have the capability of realizing high travel speed and deep penetration welding.

Come citare

Elegí el formato que necesitás y copiá la referencia al portapapeles.

APA 7

al, Y. H. E. (2018). Gas Pool Coupled Activating TIG Welding Method with Coupling Arc Electrode. https://doi.org/10.1186/s10033-018-0297-3

MLA

al, Yong Huang et. "Gas Pool Coupled Activating TIG Welding Method with Coupling Arc Electrode." 2018. https://doi.org/10.1186/s10033-018-0297-3.

Chicago

al, Yong Huang et. 2018. "Gas Pool Coupled Activating TIG Welding Method with Coupling Arc Electrode.". https://doi.org/10.1186/s10033-018-0297-3.

Harvard

al, Y. H. E. 2018, Gas Pool Coupled Activating TIG Welding Method with Coupling Arc Electrode, KeAi Communications Co, Ltd, available at: https://doi.org/10.1186/s10033-018-0297-3 [Accessed 5 Aug. 2026].

Condividi e stampa

Salva la scheda, copia il link permanente o stampala in PDF.

Esporta riferimento

Esporta il record nei formati più comuni per usarlo con un gestore bibliografico.

Dettagli della risorsa

Informazioni bibliografiche utili per verificare che sia il materiale corretto.

Titolo
Gas Pool Coupled Activating TIG Welding Method with Coupling Arc Electrode
Autore / collaboratori
Yong Huang et al
Editore
KeAi Communications Co., Ltd
Anno di pubblicazione
2018
ISSN
1000-9345
ISSN
1000-9345
Lingua
Inglés

Soggetti

Esplora risorse correlate a partire da questi soggetti.

Copiato