The effect of silk concentration on the flexural strength of FRC as a Bone Graft

Rifki Moechtar et al · faculty of dentistry universitas gadjah mada · 2018

Acceso abierto al texto completo
Lectura rápida. Revisá los datos básicos del recurso y luego accedé al contenido desde el botón principal. En esta ficha solo se muestra la información necesaria para identificar la obra, citarla y abrirla.
Publicación seriada

A Comparative microleakage analysis of two bioactive root perforation sealing materials

Esta publicación seriada contiene 501 contenidos relacionados.

Acceso al recurso

Entrá al contenido desde la opción principal o elegí otra fuente disponible.

Acceso principal

Acceso abierto al texto completo

Texto completo identificado como acceso abierto.
Abrir texto

Resumen

Descripción general del contenido del recurso.

Bone fractures are mostly caused by trauma and disease. In the therapeutic process of bone healing which often meets some constraints, bone graft is mainly used to ensure that the healing process takes place. A fiber reinforced composite (FRC) is a popular bone graft material that is made to resemble bone properties. FRC is normally comprised of polymer matrix, hydroxyapatite filler, and fiber. Hydroxyapatite is a bioactive material widely used as a bone graft. Silk fiber is known as a reliable material to increase mechanical strength of the FRC. On this basis, this study aims to determine the effect of silk fiber concentration on the flexural strength of FRC. Fiber reinforced composite made of Bis-GMA/TEGDMA/ UDMA resin (CharmFil®, DenKist, Korea), hydroxyapatite (Bioceramic Laboratory, DTMI UGM) and silk fiber (Perhutani, Pati) were divided into three groups. Each group contained different silk fiber concentrations which were 1%, 5% and 10%. The flexural strength test was performed with 3-point bending test according to ISO 10477. The result showed that FRC with silk fiber 1%, 5% and 10% respectively had flexural strength of 61.21 ± 8.43 MPa, 62.97 ± 3.92 MPa and 85.01 ± 7.71 MPa. The result of one way ANAVA analysis showed that mean of FRCs flexural strength were significantly different between one treatment group to another. Thus, it is conclusive that silk fiber has a significant effect on FRCs flexural strength. The addition of 10% concentration of silk fiber is proven to increase FRCs flexural strength.

Cómo citar

Elegí el formato que necesitás y copiá la referencia al portapapeles.

APA 7

al, R. M. E. (2018). The effect of silk concentration on the flexural strength of FRC as a Bone Graft. https://doi.org/10.22146/majkedgiind.31487

MLA

al, Rifki Moechtar et. "The effect of silk concentration on the flexural strength of FRC as a Bone Graft." 2018. https://doi.org/10.22146/majkedgiind.31487.

Chicago

al, Rifki Moechtar et. 2018. "The effect of silk concentration on the flexural strength of FRC as a Bone Graft.". https://doi.org/10.22146/majkedgiind.31487.

Harvard

al, R. M. E. 2018, The effect of silk concentration on the flexural strength of FRC as a Bone Graft, faculty of dentistry universitas gadjah mada, available at: https://doi.org/10.22146/majkedgiind.31487 [Accessed 29 Jun. 2026].

Compartir e imprimir

Guardá la ficha, copiá su enlace permanente o imprimila como PDF.

Exportar referencia

Si usás un gestor bibliográfico, podés exportar el registro en los formatos más comunes.

Detalles del recurso

Información bibliográfica útil para confirmar que se trata del material correcto.

Título
The effect of silk concentration on the flexural strength of FRC as a Bone Graft
Autor / colaboradores
Rifki Moechtar et al
Editorial
faculty of dentistry universitas gadjah mada
Año de publicación
2018
ISSN
2460-0164
ISSN
2460-0164
Idioma
eng

Materias

Explorá otros recursos relacionados a partir de estas materias.

Copiado